HCBBS Forum (English)
Submit Chemical Projects / Find Solutions
Amplify Your Requirements on a Broader Chemical Platform *Engineering · Technology · Equipment · Solutions*
Submit Request

Reddish discharge water from low-temperature boilers used in sulfuric acid production

2019-02-20View Original

Thread Content

Recently, in the low-temperature sulfuric acid production unit of our company, the boiler water turned red during blowdown, and this condition has persisted. The deaerator temperature is controlled at 100°C, and the demineralized water used is highly purified demineralized water with a conductivity of less than 0.05 us/cm. What other reasons could cause the boiler water to turn red?
Reply #22019-02-20
Is the pH value of the deionized water too low? It might be caused by acidic corrosion
Reply #32019-02-25
The deaerator temperature has been raised to 102.5℃
Reply #42019-03-02
Let’s analyze the pH value of the wastewater and the content of Fe ions in it
Reply #52019-03-02
Analyzing the oxygen content in deoxygenated water; corrosion is suspected to be caused by high oxygen levels
Reply #62019-03-03
Low deaerator temperature, inadequate deoxygenation; caused by corrosion of pipeline and boiler feed pump blades

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.