Do the inner and outer surfaces of 2507 duplex steel pressure pipes need to be pickled and passivated?

2017-11-15View Original

Thread Content

Do the inner and outer surfaces of 2507 duplex steel pressure pipes require pickling and passivation (including degreasing)? What concentration of solution should be used for treatment if necessary?
Reply #22017-11-15
Can duplex stainless steel be pickled and passivated? http://bbs.hcbbs.com/thread-120133-1-1.html (Source: Haichuan Chemical Industry Forum)
Reply #32017-11-22
It should be necessary, after all, it’s still a type of stainless steel right?:P
Reply #42017-11-25
Do the inner and outer surfaces of SAF2507 duplex steel pressure pipes require pickling and passivation (including degreasing)? Answer: Yes, it is needed. What concentration of solution should be used for treatment if necessary? Answer: The same as that of ordinary stainless steel is sufficient; however, SAF2507 duplex steel has a higher Cr content, which requires more time for pickling and passivation. For specific details, refer to AVESTA’s manual on acid washing and passivation of stainless steel surfaces.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.