Thread Content

I encountered this issue today: Pipe material: 20G; Argon arc welding is used for the root layer with ER50-6, while electric welding rods are used for the overlay layer with J427. The ER50-6 grade and J427 are not the same strength grade; so is it possible to use them together? They’re all of the same level; how come there’s one that doesn’t play by the rules? Does anyone know how the regulations specify this? So no matter how it’s combined, as long as PQR is qualified, that’s enough?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.