Regarding the selection of heat exchanger material for phosphate processing conditions

2017-12-12View Original

Thread Content

At a phosphate temperature of 30 degrees and a concentration of 25 Baumé, the volume is 60-100 cubic meters per day (over 22 hours); at a phosphate temperature of 110 degrees and a concentration of 50 Baumé, the volume is 30-50 cubic meters per day (over 22 hours). Phosphoric acid contains 500PPM of chlorine. What material should be used for a plate heat exchanger in such conditions? Thank you!
Reply #22017-12-13
Graphite heat exchangers are typically used under such operating conditions. -
Reply #32017-12-13
Suitable options include H-B, 904L, C4, h-B2, C276, Durichlor, H-G, 20CB3, 316

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.