Materials selection for resistance to sulfuric acid corrosion

2017-12-15View Original

Thread Content

With a sulfuric acid content of 1600PPM and a temperature of 120~125 degrees Celsius, which metal material is suitable?
Reply #22017-12-16
Is it a pipeline, a heat exchanger, or a tower-type device? Pipes can be made of high-silicon cast iron; for heat exchangers, graphite heat exchangers should be used, and graphite towers can also be chosen for tower-type equipment.
Reply #32018-01-04
For container types, where the pressure is relatively high, graphite is not suitable.
Reply #42018-01-04
Polytetrafluoroethylene-based anti-oxidation and corrosion coatings can be considered as a solution; they can withstand temperatures up to 250°C. They are quite convenient for pipeline installation, especially for pipelines that have not yet been installed, as they can be applied either by pouring or by brushing.
Reply #52018-01-05
What is the pressure? There are specialized graphite pressure vessels, suitable for both Class I and Class II, with a design and manufacturing grade of A4. -

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.