Consultation on hot tightening of high-temperature reactor flange bolts, as well as high-temperature pipeline flanges and valve bolts?

2017-06-28View Original

Thread Content

There is a fluidized bed reactor with a diameter of 4.6 meters and a height of 33 meters; it is made of material Q345R. The upper and lower ends of the reactor are connected via flanges. The design temperature is 420°C, while the design pressure is 0.3 MPaG. The operating temperature is 380°C, and the operating pressure is 70 KPaG. Before feeding material into this reactor, it needs to be heated to 380°C. How many times does heat tightening need to be carried out to raise the temperature from room temperature to 380°C, and at what temperatures does this take place? Additionally, for high-temperature pipelines operating at 360°C, at what temperatures must the bolts of components such as flanges, valves, and expansion joints on these pipelines be heat-tightened? Which expert can provide a detailed answer? Thank you!

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.