How to verify equipment with incomplete penetration in the longitudinal welds of cylinder welding

2017-03-27View Original

Thread Content

Our company outsourced the welding of the cylinder shells to external contractors. Previously, the company did not have any non-destructive testing equipment, so the welds were not inspected. Now, tests have shown that the longitudinal welds on the cylinder shells are not fully welded; the depth of fusion of the welds is around 1 mm on each side. For double-sided welding, there is a 1 mm unwelded area in the middle of a 3 mm thick cylinder shell. The material used is duplex stainless steel. I’m not sure how to address this issue Our operating conditions are at room temperature, with a maximum internal pressure of 3 bar, which is quite low. Could anyone with experience give me some advice? Thanks
Reply #22017-03-28
Please give some advice, everyone! Thank you so much
Reply #32017-03-30
There is under-welding that has been planed off and rewelded – what needs to be checked?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.