This post was last edited by Desert Fish on 2021-11-10 at 15:07. What causes a series of pores in submerged arc welding of pipes? Images sourced from the Internet
Reply #22021-11-10
It seems to be due to hydrogen; hydrogen is caused by the moisture in the welding materials and base metal that enters the arc zone.
Reply #32021-11-11
Are the pores dense because the welding rod wasn’t dried properly? I don’t quite understand
Reply #42021-11-15
In submerged arc welding, air currents can easily cause porosity; improper reuse of flux along with mixing it with newly used flux can also lead to such issues
Reply #52021-11-20
【Haichuan Pipeline Construction】Series of summary posts https://bbs.hcbbs.com/thread-3272979-1-1.html (Source: Haichuan Chemical Forum)
Reply #62021-11-21
The welding flux is too moist and has clumped together; The added reclaimed solder flux contains too many impurities. Affects arc stability

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.