Thread Content
The steps for starting up a catalyst in the reformation oxidation state are ( ). A. Drying, reduction, oil feeding B. Drying, oxychlorination, reduction, pre-vulcanization C. Drying, oxychlorination, reduction D. Oxychlorination, reduction, pre-vulcanization Answer: B. 5 points for a correct answer, 2 points for participation. http://bbs.hcbbs.com/thread-1495069-35-1.html Promotion of petrochemical-related activities: 1. Contest to identify sub-categories – rewarding posts available at http://bbs.hcbbs.com/thread-1568416-1-1.html (Source: Haichuan Chemical Industry Forum) 2. [Petrochemical Weekly] Issue No. 9, dated 2016-3-12 (summary of recent petrochemical activities) – available at http://bbs.hcbbs.com/thread-1568615-1-1.html (Source: Haichuan Chemical Industry Forum) 3. “Haichuan Gratitude Season” – summary of activities in the Petrochemical Section – available at http://bbs.hcbbs.com/thread-1533218-1-1.html (Source: Haichuan Chemical Industry Forum) 4. Summary of professional “basic knowledge” posts in the Petrochemical Section – supported by the main forum; great prizes await! – available at http://bbs.hcbbs.com/thread-1557057-1-1.html (Source: Haichuan Chemical Industry Forum)
B. Drying, oxychlorination, reduction, presulfurization
Select B for semi-regeneration, select C for CCR
The steps for starting up a catalyst in the reformed oxide state are ( B ). A. Drying, reduction, oil feeding B. Drying, oxychlorination, reduction, pre-vulcanization C. Drying, oxychlorination, reduction D. Oxychlorination, reduction, pre-vulcanization
B. Drying, oxychlorination, reduction, presulfurization