What to do if it rains while the chromium-molybdenum steel is being cooled after welding heat treatment?····

2016-06-07View Original

Thread Content

Dear experts, last night, a process pipeline in our factory (made of A335-P11 material) was welded, followed by post-weld heat treatment. The heat treatment process was stopped when the temperature dropped to 400°, and the pipeline was allowed to cool naturally while covered with insulation; it was around 3:15 at that time. Then, heavy rain started falling at 6 o’clock, and no shelter was installed. I’m not sure whether this constitutes quenching, and I wonder what impact it might have on the quality of my welds. Please give me some advice, thank you.
Reply #22016-06-07
Was the weld insulated at 400°? It should be fine as long as no water gets in, right?……
Reply #32017-04-14
Heat treatment itself does not reach the temperature at which phase transformation occurs; limiting the heating and cooling rates is mainly to prevent the generation of new stresses

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.