GB/T3077-2015 is about to come into effect, and this standard eliminates the grades marked with a ‘A’. For example, 35CrMoA in GB150 becomes 35CrMo in GB/T3077-2015; should it therefore be denoted as 35CrMo according to the new standard?
Reply #22016-08-21
It should be labeled according to the new standards...
Reply #32016-08-22
Use the appropriate standard and indicate it accordingly!
Reply #42016-08-29
I see now; GB/T3077-2015 also lists 35CrMoA, and it should be designated using the grade specified in GB150
Reply #52016-08-29
What do you write for the bolt standard when making the notation? Write 150? Write 3077? Neither, it should be written as HG/T20613; and according to standard 20613, it is 35CrMo, so. . . Actually, there’s no need to worry about it; such things have no real impact.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.