Heat exchanger tube sheet, 16MnR overlay welding ER2209, do I need an over-layer welding rod? If necessary, is it better to use A302 or A402?
Reply #22016-11-13
It is recommended to add a transition layer, welding rod A402
Reply #32016-11-13
This post was finally edited by qwl on 2016-11-13 11:46 to recommend transition layer, welding rod A302 heat exchanger tube plate surfacing process http://wenku.baidu.com/link?url= ...naTpaYFQsSLFbdMziSq
Reply #42016-11-13
The transition layer is needed, otherwise it will be easy to corrode near the weld.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.