A large number of interface cracks appeared after welding of HDPE polyethylene pipes on the construction site

2017-05-15View Original

Thread Content

I found out the reason and guessed that the welding temperature of the workers was too high, which should not exceed 220 degrees Celsius. I would like to ask, what will happen if the HDPE exceeds 220 degrees Celsius?
Reply #22017-05-15
The welding speed is too fast, the base material does not melt and the welding wires do not melt each other.
Reply #32017-05-16
The temperature is over 230. Reached 250. Does it also have an impact on the quality of butt welding?
Reply #42017-05-16
PR hot melt butt welding does not require welding rods.
Reply #52017-05-16
It will also have an impact. If the temperature is too high, changes in material properties will occur.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.