HCBBS Forum (English)
Submit Chemical Projects / Find Solutions
Amplify Your Requirements on a Broader Chemical Platform *Engineering · Technology · Equipment · Solutions*
Submit Request

Combined process qualification

2017-09-08View Original

Thread Content

May I ask, should bending tests be conducted on the test specimens for combinations where T<10mm? If it is to be done, what kind of bending test should be carried out?
Reply #22017-09-08
So, may I ask, is it scoliosis, facial distortion, or back curvature?
Reply #32017-09-08
Table 11 of NBT47014-2011
Reply #42017-09-09
For sizes below 10mm, it is not recommended to conduct combined process evaluations; it is difficult to select appropriate bending specimens, as neither face bending nor back bending nor side bending is suitable. There was a dedicated thread previously discussing this issue, and some people suggested doubling the number of samples for face bending and back bending. The original poster can look that up
Reply #52017-09-09
For combinations of less than 10, evaluate by performing face and back bending. ,。

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.