The acid metering tank has been in use for 3 years, and its lower part is corroded; what should be done now?
Reply #22018-07-05
Is it sulfuric acid? Re-welding will do, but be careful about safety
Reply #32018-07-06
Is there a rubber lining layer inside this?
Reply #42018-07-06
Is there a rubber lining layer inside this?
Reply #52018-07-06
A heating tape was used; it’s probably concentrated sulfuric acid. If that doesn’t work, replace it with a metering tank lined with steel and PE – it’s inexpensive and durable
Reply #62018-07-06
After being treated with Teflon for corrosion protection, it will not corrode or wear through
Reply #72018-07-07
30% hydrochloric acid: external welding has been used, along with an internal method; the interior part is reinforced with fiberglass, while the outer layer is coated with resin

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.