What to do if the chloride ion level is too high during the on-site hydrostatic test of stainless steel storage tanks?

2025-04-16View Original

Thread Content

For on-site stainless steel storage tanks, when there is no deionized water available for the hydrostatic testing and the chloride ion concentration exceeds 25 ppm, what is the usual approach to deal with this situation?
Reply #22025-04-16
See 150.4-2024 11.4.2.1 for details
Reply #32025-04-17
If there is truly no water that meets the standards, it can be used temporarily to complete the pressure washing; after that, the area should be drained and cleaned thoroughly before rinsing it with deionized water using a high-pressure water gun. Make sure to rinse thoroughly. In this way, only a small amount of deionized water is needed, so it should be easy to obtain
Reply #42025-04-17
I didn’t notice any new statements regarding the standards; I studied * it

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.