Can 2205 tubes be expansion-welded to 316L tube sheets?

2019-04-09View Original

Thread Content

Gentlemen, the material of the 2205 pipe is hard; it’s 25X1 in size. Can it be expansion-welded to a 316L tube sheet with sufficient strength? If expansion joining was possible, did the tube crack during the expansion joining process? How is the equipment performing? Thank you
Reply #22019-04-09
Thank you. May I ask what the pipe specifications are, and did the pipes crack during expansion joining?
Reply #32019-04-09
Building】 Thank you. May I ask what the diameter of the pipes is, and did the pipes crack during expansion? How is it working?
Reply #42019-04-10
It’s best not to use expansion jointing; you can take a look at an article on the Haichuan Corrosion Technology Forum, especially in environments with chloride ions
Reply #52019-04-11
Thank you. Setting aside electrochemical corrosion and intergranular corrosion caused by different materials, from the perspective of manufacturing processes and performance, can 25x1 2205 tubes be welded to 316L tube sheets?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.