Measures to prevent intergranular corrosion and pitting in A-type SS

2026-01-18View Original

Thread Content

Intergranular corrosion: Avoid heating A-type SS in the range of 500–800°C, or perform solution treatment again after heating. Use SS containing sufficient amounts of Ti and Nb, or add a stabilization treatment. Ultra-low carbon or high-purity A-type SS, duplex SS are used. Pitting: SS with a high chromium content, or those containing large amounts of alloying elements such as Mo, N, Si, etc., – duplex SS. High-purity SS is used to improve surface finish. Amorphous corrosion-resistant alloys – eliminating various defects inherent in crystalline alloys (grain boundaries, dislocations, segregation, etc.)

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.