For water cooler tube bundles as well, the anti-corrosion effects differ between those with and without anti-corrosion treatment

2026-04-12View Original

Thread Content

The images below show the top rear cooler of the distillation column (diameter 1300) in a petrochemical company’s heavy oil catalytic unit, as well as the rear cooler for gasoline products in the stabilizer unit; in both cases, the same circulating water was used for 3 years.
Reply #22026-04-12
Generally, anti-corrosion treatment on the carbon steel surface on the circulating water side yields good results

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.