Cold tightening amount of steam pipes

2017-11-02View Original

Thread Content

t=430℃, p=3.5MPA, steam pipeline, 15CrMoG, SH/T3405, Sch80; cold straining of the pipeline with a coefficient of 0.7 – the amount of cold straining between the two fixing points reached 100 mm. No actual cold straining has been carried out yet. May I ask everyone, is it easy to carry out the construction on site? Is there any experience regarding on-site construction regarding what a suitable cold tightening value is?
Reply #22017-11-02
DN200 pipeline, GB5310

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.