What to do if the SCR catalyst module is partially exposed to rainwater

2021-06-17View Original

Thread Content

The catalyst module has been installed in place; a small amount of rainwater entered due to the heavy rainfall. What should be done regarding drying the furnace after one week?
Reply #22021-06-17
Can controlling the furnace temperature at 200 degrees for one hour while heating it solve the problem?
Reply #32021-06-22
Keep the furnace temperature at 150 degrees, bake for 24 hours, and it’s ready once the moisture level meets the requirements

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.