Can the chlor-alkali industry use 316L material for refining once and twice saturated brine at a temperature of 40 degrees?

2022-07-20View Original

Thread Content

Can the chlor-alkali industry use 316L material for refining once and twice saturated brine at a temperature of 40 degrees? What materials do you use?
Reply #22022-07-20
Can duplex steel be used 2205 2207 etc.
Reply #32022-07-20
If the temperature is not high, what are these pipes used for? Non-metallic ones are much better.
Reply #42022-07-20
316L So much sodium chloride won’t corrode it?
Reply #52022-07-20
316L is resistant to chloride ion corrosion
Reply #62022-07-21
The pipes are made of CPVC material.
Reply #72022-08-15
You can choose anti-corrosion coating, which is more cost-effective
Reply #82022-08-17
It is better to choose titanium or lined carbon steel for refined brine, because in refined brine, due to fluctuations in process operations or lax removal of active chlorine in previous processes, hypochlorite can enter the refined brine, which can be very detrimental to stainless steel.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.