【Daily Question】Multiple-choice question 11.9: When sulfiding a general hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value,

2015-11-09View Original

Thread Content

Generally, when sulfiding a hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value, the sulfidation rate no longer increases. Generally, when the H2S concentration in the circulating hydrogen reaches (), the sulfur injection rate can be appropriately reduced. A. 0.5% B. 1.0% C. 2.0% D. 3.0% B
Reply #22015-11-09
Generally, when sulfiding a hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value, the sulfidation rate no longer increases. Generally, when the H2S concentration in the circulating hydrogen reaches (B), the sulfur injection rate can be appropriately reduced.
Reply #32015-11-09
Generally, when the H2S concentration in the circulating hydrogen reaches (B), the sulfur injection rate can be appropriately reduced.
Reply #42015-11-09
B, 1.0%------------------------------------------------------------------
Reply #52015-11-09
Generally, when sulfiding a hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value, the sulfidation rate no longer increases. Generally, when the H2S concentration in the circulating hydrogen reaches (B 1%), the sulfur injection rate can be appropriately reduced.
Reply #62015-11-09
The answer is C; it is generally between 0.2% and 2%
Reply #72015-11-09
Generally, when sulfiding a hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value, the sulfidation rate no longer increases. Generally, when the H2S concentration in the circulating hydrogen reaches (B, 1.0%), the sulfur injection rate can be appropriately reduced.
Reply #82015-11-09
Generally, when the H2S concentration in the circulating hydrogen reaches (B), the sulfur injection rate can be appropriately reduced.
Reply #92015-11-09
Generally, when sulfiding a hydrogenation catalyst, once the H2S partial pressure in the recycle hydrogen reaches a certain value, the sulfidation rate no longer increases. Generally, when the H2S concentration in the circulating hydrogen reaches (B), the sulfur injection rate can be appropriately reduced. A、 0.5% B、 1.0% C、 2.0% D、 3.0%

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.