Difference in materials

2016-01-14View Original

Thread Content

Hello, fellow marine engineers. I work in the field of hydrogenation processes, and I have a question for you: what is the difference between 2.25Cr1Mo and 12Cr2Mo1 in chromium-molybdenum steel? These materials are often used in reactors, and I’m not quite sure what the differences are; what are their advantages and disadvantages? Thank you all; please feel free to share your advice! ! !
Reply #22016-01-14
The explanation on the first floor was excellent; 12Cr2Mo1R can be used as a substitute for SA387GR22CL2.
Reply #32016-01-14
We all use 15CrMoR; it seems that 12Cr1Mo can achieve higher performance than it, but I’m not sure about the other options
Reply #42016-01-14
2.25Cr-1Mo is the designation in American standards. That is, the pile of materials P22 F22 B22 FP22 T22 inside. .
Reply #52016-02-22
Does anyone know where I can buy this type of steel plate, with a diameter of around 2 meters and a thickness of about 11 cm?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.