Seeking help with a welding process issue regarding C276+16Mn

2016-03-19View Original

Thread Content

There is currently a Hastelloy C276 composite plate equipment; the flat cover has several connections, with a wall thickness of around 3–5 mm, and the thickness of the flat cover itself is about 50 mm, featuring a fully penetrated structure; May I ask what kind of plate butt weld assessment is required to cover this? Thank you.
Reply #22016-03-19
Won’t this plug-in type leak during welding?
Reply #32016-03-20
More than 2 weld evaluations may be required, 1 thin + 1 thick
Reply #42016-03-20
If it’s a fillet weld, isn’t the thickness range unrestricted?……

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.