HCBBS Forum (English)
Submit Chemical Projects / Find Solutions
Amplify Your Requirements on a Broader Chemical Platform *Engineering · Technology · Equipment · Solutions*
Submit Request

【Daily Question】20160421 Coating thickness of composite tube sheets (top 50 participants + 2 bonuses)

2016-04-21View Original

Thread Content

This post was last edited by humanrzm on 2016-4-25 08:38. To increase the popularity of the heat exchange forum, a \"Question of the Day\" activity has been introduced there; this helps to foster an active atmosphere for technical exchanges while also providing members with financial rewards. 【Daily Question】True or False: According to standards, for composite tube sheets welded to heat exchange tubes, the thickness of the coating layer should not be less than 3 mm. ( ) Answer: Correct; for details, see GB/T151-2014, clause 7.4.2.3. Other content: AC version of heat exchange equipment – “One question per day” competition post (prizes for participation; valid indefinitely) http://bbs.hcbbs.com/thread-1320941-1-1.html “【Mechanical Section】Recruitment for moderators & technicians; applications and referrals are welcome【Valid indefinitely】If you’re interested, come ahead! 】http://bbs.hcbbs.com/thread-1568748-1-1.html 【Mechanical Section】Call for collection of essential knowledge articles http://bbs.hcbbs.com/thread-1389197-1-1.html Haichuan’s “Thanksgiving Season” sharing event http://bbs.hcbbs.com/thread-1579172-1-1.html
Reply #22016-04-21
True or False: Standards specify that for composite tube sheets welded to heat exchange tubes, the thickness of the coating layer should not be less than 3 mm. (Incorrect) Please refer to 6.6.3.2 and 6.6.3.3 in GB/T151-2014; this requirement applies only when expansion joints are used for strength welding.
Reply #32016-04-21
True or False: Standards specify that for composite tube sheets welded to heat exchange tubes, the thickness of the coating layer should not be less than 3 mm. ( √ ) For details, see Clause 7.4.2.3 of GB/T151-2014.
Reply #42016-04-21
The standards specify that for composite tube sheets welded to heat exchange tubes, the thickness of the coating shall not be less than 3 mm. (Correct)

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.