Reply #22016-05-06
Strictly control the effect of the rough separation process and maintain a stable flow rate of gas entering the fine separation stage; the key is to manage the moisture content in the gas
Reply #32016-05-07
We require that the sulfur content in the dew point remover be less than 0.1 ppm; strict control is applied to this parameter, and the gas supply is immediately cut off if the limit is exceeded. There is online analysis at the low-temperature methanol washing outlet. The sulfur capacity of the absorbent in the distillation tower should be tested regularly. The amount of high-pressure steam added should be appropriate
Reply #42016-05-10
In addition to the regular regeneration of the degreasing tank, pre-hydrogenation can be regenerated using high-temperature steam, with strict control over the amount of hydrogen sulfide entering and the ammonia content
Reply #52016-05-10
In addition to the regular regeneration of the degreasing tank, pre-hydrogenation can be regenerated using high-temperature steam, with strict control over the amount of hydrogen sulfide entering and the ammonia content

Submit a Project

Need technical support or have a project requirement? No registration needed.

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.