Does the minimum forming thickness include a corrosion margin?

2016-06-24View Original

Thread Content

Minimum forming thickness: The minimum thickness required after forming the compressed component to meet the design specifications. Does it include a corrosion margin?
Reply #22016-06-24
The last edit to this post was made by zdl1966 on 2016-6-24 at 12:14. Should Article 4.3.7 of GB150.1-2011 stipulate that the minimum thickness of the shell after processing, without taking into account any corrosion allowance or negative deviations in the steel plate thickness, be as follows:
Reply #32016-06-24
The formed thickness includes the corrosion margin C2, that is, the nominal thickness minus C1 and C3

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.