Selection of drying conditions for hydrogenation refining catalysts

2016-09-02View Original

Thread Content

Dear sea friends, there’s a question I haven’t been able to figure out: why is the drying of hydrogenation refining catalysts carried out at constant temperatures of 120°C and 250°C? I hope my friends can provide an answer; thank you very much
Reply #22016-09-02
One is the removal of free water (low temperature). One is dehydrated molecular water (structural water)
Reply #32016-09-13
250℃ is probably the condition for thermally tightening pipeline valves
Reply #42016-09-17
We specialize in the recycling of waste catalysts, as well as various non-ferrous metal wastes containing copper, zinc, nickel, molybdenum, platinum, palladium, etc. We possess a license for handling hazardous waste and have all the necessary environmental compliance certifications. Manufacturers and individuals who are in need can contact Manager Zhang at 13203847799

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.