Forged from MonelK500; fractures and cracks occur during the final processing of the product

2016-11-26View Original

Thread Content

MonelK500 is forged, and fractures and cracks occur during the finishing process of the finished product – is this simply a problem arising from the heat treatment process? There are no issues with the ingredients or raw materials
Reply #22016-12-04
So, is there a big difference between Monel 400 and MONEL K500? Can one replace the other? If 400 is used in place of 500, the problem should not be serious, right?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.