Problems with flange mechanical performance testing

2020-08-17View Original

Thread Content

We have a purchase plan for flanges made of HC-276 material. The customer requested that the flange material and mechanical properties be inspected. However, the supplier's flanges are made of steel rods. The supplier responded that the mechanical properties are guaranteed to be qualified when used longitudinally (2 in the picture below), but the mechanical properties are not guaranteed to be qualified when used horizontally (1 in the picture below). Is this the case? When testing mechanical properties it will definitely be transverse.
Reply #22020-09-11
The test has been completed. After the steel rod is cut, it will be solution treated and the processed flange will meet the requirements.
Reply #32020-09-11
Find ways to meet customer needs, like it

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.