GB150 specifies that containers with undercutting are not allowed, including those made of CrMo low-alloy steel. I wonder why the standard mentions low-alloy steel
Reply #22017-10-31
When welding low-alloy structural steel, the edge of the undercut becomes hardened, and due to stress concentration, it often becomes a cause of welding cracks.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.