The welded H-beam has cracked

2017-09-08View Original

Thread Content

Web thickness: 24 mm; Flange thickness: 40 mm. Material: Q345B. Welding method: Submerged arc welding
Reply #22017-09-08
Made of Q345B material with a relatively thick plate thickness; welding without preheating may result in cracks.
Reply #32017-09-08
The steel plate is too thick, resulting in high structural stiffness and large welding stresses. Preheating, wire energy control, and heat treatment after welding are advisable.
Reply #42017-09-08
The structural stiffness is too high; for such welding, preheating and staged welding in sections are required
Reply #52017-09-09
The thickness of the web and flanges is different, resulting in high stress in the fillet welds. When using submerged arc welding, the welding heat input is relatively high; therefore, attention must be paid to the welding process parameters

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.