Has Haiyou used hot-rolled composite plates? Can a batch of 2205+Q235B plates for evaporation separation chambers, with a pressure of -0.08 and a temperature of 130 degrees, be used in a negative-pressure environment? Give some advice
Reply #22020-07-15
It was used a long time ago; at that time, the rolling technology wasn’t advanced enough, which made it very easy to end up with two layers of material. Later on, explosive bonding was used instead. Now that the new standards incorporate rolled composites, the adhesion rate and shear strength should be fine, right? The technical level has improved significantly, hasn’t it?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.