When using composite plate equipment, how is the coating thickness determined?

2020-10-26View Original

Thread Content

How is the coating thickness determined when using composite panel equipment?
Reply #22020-10-26
Depending on the degree of corrosion, it should be no less than 3 mm at minimum.
Reply #32020-10-26
After lamination, the general consideration is medium compatibility; corrosion margin is basically not taken into account! Why choose laminated instead? The thickness can be determined according to the requirements of the processing technique! You request 1mm, but manufacturing technology imposes limitations!
Reply #42021-01-04
Why 3 millimeters? The composite panels that were subjected to blasting in the past were 2 millimeters thick
Reply #52021-01-04
The composite layer can resist corrosion as long as it exceeds a minimum thickness; however, it does not enhance performance and instead increases the difficulty of compounding. An excessively low thickness is not conducive to manufacturing, especially when welding is required, as it hinders the welding joints of the composite sheet

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.