Why is the separation of nickel in P507 not good?

2020-04-29View Original

Thread Content

Nickel-cobalt separation: Why is P507 not effective for nickel separation? After purification with P204, the pH of the solution is between 4.0 and 4.5; the concentration of cobalt is 30–35 grams per liter, that of nickel is 1–2 grams per liter, and that of magnesium is 3–5 grams per liter. The organic concentration of P507 is 20%, while the saponification rate is 60–65%. The flow rate in the washing stage is high, and the magnesium concentration has been reduced to below 0.002 grams per liter. Then why is there still nickel present in the back-extraction stage?
Reply #22020-10-28
Bro, have you found out what the problem is? I’ve run into this problem too
Reply #32020-12-14
There is usually a trace amount of entrainment, and the nickel carried along can be washed away through the nickel washing stage.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.