Roughness of paint coating surfaces and its causes

2026-02-18View Original

Thread Content

After the paint film dries, irregularly shaped raised particles are distributed on its entire or partial surface. Surface roughness is essentially the result of an imbalance among four factors: the substrate, the material, the manufacturing process, and the environment; it is by no means due to a mistake in just one aspect. Priority should be given to three aspects: substrate cleanliness, paint filtration, and standardization of spraying parameters; over 90% of problems can be avoided in advance ; If it has already occurred, mild cases can be repaired using sandpaper and polishing; for severe cases, it is recommended to redo the work to ensure durability.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.