How can I reduce the amount of arsenic-containing matte? Experts, please give me some suggestions

2017-08-07View Original

Thread Content

Our furnace is used to process copper slag; the arsenic content in this slag is about 7 times higher. The amount of matte and red matte produced each time is very small, while white matte (arsenic-containing matte) accounts for 60% of the total output. What can be added to reduce the amount of arsenic-containing matte? I seek advice from experts
Reply #22021-03-25
I have been studying this problem for a long time, but I still haven’t found any effective solution. Theoretically, increasing the sulfur content in copper slag can reduce the production of arsenic-containing matte. From a phase perspective, arsenic-containing matte exists in the form of copper arsenide and metallic copper; copper arsenide is difficult to handle, but metallic copper can be converted into matte by increasing its sulfur content. In production practice, adding pyrite during ingredient preparation yields no significant effect.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.