Corrosion issues with mixed acids

2021-06-16View Original

Thread Content

Does a mixture of 98% concentrated sulfuric acid and 65% concentrated nitric acid corrode stainless steel at room temperature? If there is any, what material would be better!
Reply #22021-06-16
Using a carbon steel lining with PTFE or another type of adhesive can solve the problem.
Reply #32021-06-17
It is better to use steel skeleton composite pipes when the temperature does not exceed 100°C
Reply #42021-06-18
The fluoroplastic-lined pipes we use are still fine for now
Reply #52021-06-19
PTFE lining can handle temperatures of 150°C; for 180°C, PFA lining can be used, and for even higher temperatures, Hastelloy should be considered
Reply #62021-06-27
If the temperature exceeds 200 degrees, use zirconium materials directly; it’s just a bit expensive

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.