In coal tar hydrogenation, the pressure difference is high; the water injection volume needs to be increased. How to address the situation where the pressure difference doesn’t decrease?

2018-01-15View Original

Thread Content

This post was last edited by liaifeng on 2018-8-5 11:00. How to handle it?
Reply #22018-01-16
What is exchanging heat with what, is coking occurring? Increase the number of bypasses to see if there is an improvement
Reply #32018-01-16
Scaling and ammonium salt crystallization lead to high pressure differences in heat exchangers
Reply #42018-01-16
Use a polymerization inhibitor to prevent scaling; water should be injected before the heat exchanger, and the temperature before heat exchange must be above 240 degrees. Monitor chloride ions as well

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.