What is the control range for the reaction temperature in hydrocracking? .
Reply #22018-11-01
Generally, the cracking bed layer does not exceed 427℃
Reply #32018-11-01
It depends on things like operating conditions and catalyst activity, I guess
Reply #42018-11-06
For the wax oil hydrogenation process, the operating temperature in the refining reactor is 360–390 degrees, while it is around 400 degrees in the cracking reactor. Provided that the nitrogen content in the refined oil remains within acceptable levels, the lower the reaction temperature, the better

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.