When welding with NS312 electrodes, what can be done to address the issue of persistent lack of fusion? Is there any good way?

2019-10-11View Original

Thread Content

When welding with NS312 electrodes, what can be done to address the issue of persistent lack of fusion? Is there any good way?
Reply #22019-10-11
Welding method, welding current, welding speed
Reply #32019-10-11
For this case, it’s better to choose TIG welding.
Reply #42020-03-10
Base material thickness: Non-fusion refers to either interlayer non-fusion or inter-pass non-fusion. It’s necessary to reflect clearly in order to make a judgment.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.