How to perform the temper embrittlement tendency assessment test with stepped cooling

2015-07-14View Original

Thread Content

For the evaluation of temper embrittlement tendency, there are 16 groups each for the weld metal and the heat-affected zone, with 3 specimens in each group. 8 groups with stepped cooling. So for this test, does the length of the test plate have to be 10*16*3=960? What does stepped cooling mean? How is it implemented exactly? For the process, does one just need to decide the length of the test plate, and nothing else needs to be considered?
Reply #22015-07-14
The machining allowance at the notch of the impact specimen needs to be considered. Moreover, 16 groups of samples may be sufficient or insufficient (the randomness in impact energy values can be quite high). It’s better to prepare as many samples as possible.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.