For Q345R, which is available in hot-rolled, controlled-rolling, or normalized heat-treated conditions, what is its main microstructural pattern? What is the organizational proportion?
Reply #22015-08-19
Base metal: Ferrite + Pearlite
Reply #32015-08-19
The microstructure of Q345R consists of ferrite and pearlite; the pearlite content in the normalized state is higher than that in the hot-rolled state
Reply #42015-08-19
The answer above is correct; at room temperature, its microstructure consists of ferrite + pearlite, that is, cementite
Reply #52015-08-20
Q345R is a hypoeutectoid steel, and its microstructure at room temperature consists of ferrite + pearlite
Reply #62015-08-20
The microstructure of Q345R consists of ferrite and pearlite
Reply #72015-08-20
It was originally thought to be ferrite. I checked later and it was ferrite + pearlite. From the microstructure diagram, there is more ferrite, accounting for about 80-90%, I’m not sure if that’s correct. Thank you all for your help.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.