Problems in opening thick-walled composite panels

2015-10-19View Original

Thread Content

Risks to be considered during the manufacturing of composite Q345R 100+3 pipe fittings with dn200 insert-type connections
Reply #22015-10-19
The weld seam must be ground to make the interior smooth. If the plate is thick while the fitting is thin, it may damage the fitting during welding.
Reply #32015-10-19
Penetration welding and ultrasonic testing are generally required. The takeover groove is preferably machined, with a double-sided U-shaped groove; welding heat input should be controlled, and interpass cleaning is necessary.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.