0Cr13 welding process

2015-11-03View Original

Thread Content

This post was last edited by Menghan100 on 2015-11-5 at 18:34. Do any experts have any pre-welding procedures for 0Cr13+Q345R composite sheets? Urgent! Praise be to God!
Reply #22015-11-03
Reference can be made to clause 9.1.78 in NB/T47015-2011: http://bbs.toweld.com/images/post/smile/default/smile.gif
Reply #32015-11-03
Thank you:handshake:handshake:handshake:handshake:handshake:handshake:handshake:handshake:handshake:handshake:handshake
Reply #42015-11-03
Austenitic electrodes are used for both the transition layer and the clad layer. A302+A102
Reply #52015-11-05
Thank you very much for your reply:handshake:handshake:handshake:handshake:handshake

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.