For concentrated hydrochloric acid, the PTFE-lined magnetic flap – why does the lining layer deform? Used for 5 years, with insulation but no heat tracing. The equipment is a atmospheric pressure tank; I want to know what caused the deformation of the lining
Reply #22018-08-29
What is the temperature? The use of tetrafluoride should preferably not exceed 100, as it is prone to creep and deformation.
Reply #32018-08-31
It’s best to take a photo, as well as to note any abnormal production conditions that may occur on a daily basis, such as changes in temperature or the presence of negative pressure And how thick is the PTFE lining? It is necessary to examine the reasons from various aspects, as well as to determine whether it is PTFE Could it be other materials such as polyethylene?
Reply #42018-09-03
Today, it was decided that the lining material will be rubber, not PTFE
Reply #52018-09-27
It’s normal for there to be deformation after five years; it shouldn’t be too severe. That’s what rubber linings are like.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.