Manufacturing of pressure vessel cylinders

2019-06-04View Original

Thread Content

What are the methods for designing and manufacturing pressure vessel shells? What is the typical thickness of sheets that can be rolled by a sheet rolling machine? For the thickness, a wound structure can be adopted; what are the requirements regarding the axial stress in a wound structure? With thicknesses of 30 mm and 100 mm respectively, what structural form should be adopted? Please give me your advice
Reply #22019-06-04
The maximum thickness of the coiled sheet at present is 120 mm
Reply #32019-06-04
Thank you, do you know anything else?
Reply #42019-06-05
For those with a smaller diameter, seamless steel pipes can be used directly.

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.