Thermal melt salt storage tank: issue of 100% RT X-ray inspection for the butt joints of the mid-gusset plates in the entire edge plate

2021-02-01View Original

Thread Content

This tank operates at a high temperature of 400 degrees, and the entire tank is to be scanned with X-rays 100%. I’m wondering how to attach the film to the bottom of the tank; my idea is to raise it to a height of 800–1000 units, use TIG welding for the base layer and electric welding for the top layer. Is this approach feasible? I really don’t know how to take photos of those with a diameter of 30 meters. Please share your opinions so we can learn from each other*
Reply #22021-02-02
Bottom plate? ? ? Are all butt welds of this type?
Reply #32021-02-02
Yes, it’s a butt joint; the edge plates are arc-shaped, not bow-shaped. No flat strips are used in the butt welds, and all of the mid-section plates of the edge plates are joined by butt joints. X-ray – how should the film be placed?

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.