The holes in the tube sheet are too close to the edge – is it still usable?

2021-03-27View Original

Thread Content

The holes in the tube sheet are too close to the edge – is it still usable?
Reply #22021-03-27
It doesn’t matter if one tube is missing; just block it off.
Reply #32021-03-27
It can be used; the pipe is 2 millimeters lower than the tube sheet, and welding or expansion joining can be used
Reply #42021-03-27
1. Can it be welded? 2. What is the operating condition?
Reply #52021-03-28
Suitable for corrosive materials at non-high temperatures
Reply #62021-03-28
We’ve encountered the same problem too; yours is further to the side than mine
Reply #72021-03-29
In the case of tube expansion, it can be used with somewhat decent skills, but it is not recommended. This is because the tube sheet and the edges of the shell are areas where stress changes are significant, making it easy for leakage points to form; it is advisable to seal those areas instead
Reply #82021-03-29
It has a hole on top and its flange sealing surface has already been attached; it should be difficult to pass a pipe through it

Submit a Project

**Looking for Chemical Technology, Equipment & Solutions?** No Registration Required Broader Platform Exposure | Global Chemical Service Provider Connections

Submit Request — Free Consultation

Disclaimer

This is an automated machine translation of the original thread. Some technical terms may have inaccuracies; the original text shall prevail. Click "View Original" at the top right to access the source page, which supports IP-based automatic real-time language translation. Please watch out for contact details and sales inducements to prevent fraud. All content and translations are for reference only, representing solely the poster's personal views. For enquiries, email service@hcbbs.com.